I only have experience with horizontal roller hearth tempering lines .
I received recently a comment that anisotropy was less conspicuous in the old days when produced on vertical (hung) tempering... |
|
|
Glass coverage in vehicle is expending due to panoramic roof, high rake angle of windshield and Cielo design.
As the coverage expend, the heat/light transfer through glass is more imfortant.
And... |
|
|
We are a leading manufacturer of the Eva Film in China. Laminated glass is laminated by Eva Film or Pvb Film. However, Eva Film is much cheaper than Pvb Film. And it is easily to be operated. So more... |
|
|
WHY DO WE USE STRUCTURAL BONDING TAPE? |
|
|
Hi, everyone. I'm designing a glass lift enclosure. I understand some air pressure will be induced by the lift car movement. without testing, can i estimate the air pressure by calculatioon? |
|
|
This is a special, patented, technology that incorporates LEDs ,light sources or Electronics materials into glass panels to create distinctive patterns, images and logos. It performs as an excellent p... |
|
|
Hello, I am inquiring on what spacer materials glass manufacturers are using for their transportation needs as spacer and button pads? Can any of you reply out there?
Recently with the spike $-vs-Eu... |
|
|
Laminated glass is made by two or more than two pieces glass, PVB film was between the glass and glued the glass under high temperature and pressure. Laminated glass is necessary equipment for making... |
|
|
It’s regarding glass re-tempering. We are currently doing this process and I am wondering if this is advisable. We are doing this since there are times there’s a slight waviness in the glass after... |
|
|
We'd enjoy contributing designs and artwork for execution is glass designs, for example frit designs on solar panels, and other translucent prototype design concepts.
Thanks for considering!
T... |
|
|
We are producing and supplying the extra clear glass for solar ,and solar glass now .
The size of solar glass 1650x2440, 2mm,3.2mm,4mm.
The size of extra glass 1830x2440,3300x2134, 2mm-19mm
If... |
|
|
Is there a formula out there to figure what temperature glass needs to be brought to before quenching for tempering? i've looked and looked, and asked around, but all i've found so far is that its a... |
|
|
so we bot this machine and set it up supposedly being able to do 3mm glass. well, so far, as long as we don't exceed 30" x 60", we're good. thats not good enough. we're successful so far in trickin... |
|
|
Can anyone shed any light on the DIN 50049 standard that is part of DIN18516 as details of this standard and copies of this standard are referred to but the actual standard seems to not exist in paper... |
|
|
Have you seen motion pictures Transformer? You like it? <a href=" http://www.sinotrailers.com/self-propelled-modular-transporters.html" title="SPMTs">SPMTs</a> is something like that. You can transfor... |
|
|
I am looking for a product that will offer a greater degree of restistance to scratching graffiti on heat tempered glass. Prefably the process will be post-production (coatings and/or chemical treatme... |
|
|
I am in requirement of a resin or a gel to fill up areas between two glass sheets.
Can anyone pleas inform what resin or gel can be used. There should be no bubble formation and also the resin shoul... |
|
|
Dear Sir
How are you!
i am very glad to know you.from the internet,i know your company is interesting in building material company and need to import the float glass .
i am very gl... |
|
|
Dear Sir
How are you!
i am very glad to know you.from the internet,i know your company is interesting in building material company and need to import the float glass .
i am very gl... |
|
|
Privacy glass is designed by principles of polymer liquid-crystal optics. In the natural state, liquid crystal droplets are aligned randomly in the polymer and the reflective index of liquid crystal d... |